QuantaPreg® PrePreg
Product Description
QuantaPreg® was performed by using the TPU (Thermoplastic Polyurethane) Resin as base for pre-impregnation, multi-layers were reinforced for prepreg. It’s essential raw material of high-performance composite reinforcement.
UHMWPE has the highest strength-to-weight ratio among high performance fibers and the best impact-resistance. It has density of 0.97g/m³, the lightest among reinforcement fibers, its tensile strength value 45cN/dtex weighs 2/3 of aramid fiber and only half of carbon fiber. Therefore, fabric made with UHMWPE is not only light but also has excellent tensile strength and tear strength. UHMWPE fiber is flexible and absorbs energy during plastic deformation. Its ability to absorb 1.8 times of carbon fiber, 2.6 times of aramid fiber and 33 times of E-glass fiber.
QuantaPreg® PrePreg has excellent mechanical properties, it helps end-product gain higher strength, lightweight, higher modulus and flexibility, also exceptional impact and puncture resistance. TPU can undergo secondary thermos-plasticization and can be composited with high-performance fiber prepreg such as fiberglass and carbon fiber to lay laminated boards.
Properties
- Excellent mechanical properties
- Optimized impact resistance
- Optimized Puncture Resistance
- Improved the toughness
Technical Data Sheet
单位 UOM | QuantaPreg® | 检测标准 Test standard | |
---|---|---|---|
面密度 Areal Density | g/m² | 120±10 | GB/T4669-2008 |
厚度 Thickness | mm | 0.2±0.05 | GB/T3820-1997 |
拉伸强度 Tensile Strength | N/5cm | ≥2000 | GB/T3923.1-2013 |
≥1800 | |||
断裂伸长率 Elongation | % | ≤ 10 | GB/T3923.1-2013 |
≤ 10 |
PrePreg Technical Data Sheet
单位 UOM | QuantaPreg® | 检测标准 Test standard | |
---|---|---|---|
面密度 Areal Density | g/m² | 120±10 | GB/T4669-2008 |
厚度 Thickness | mm | 0.2±0.05 | GB/T3820-1997 |
拉伸强度(经向) Tensile Strength(经向) | N/5cm | ≥2000 | GB/T3923.1-2013 |
拉伸强度(维向) Tensile Strength(维向) | N/5cm | ≥2000 | GB/T3923.1-2013 |
断裂伸长率(经向) Elongation(经向) | % | ≤ 10 | GB/T3923.1-2013 |
断裂伸长率(维向) Elongation(维向) | % | ≤ 10 | GB/T3923.1-2013 |
技术参数表
检测项目 | 测试标准 | 测试结果 | |
---|---|---|---|
克重 g/㎡ | GB/T4669-2008 | 120±10 | |
厚度,mm | GB/T3820-1997 | 0.2±0.05 | |
断裂强力 N/50mm | 经向 | GB/T3923.1-2013 | ≥2000 |
纬向 | ≥1800 | ||
断裂伸长率 % | 经向 | GB/T3923.1-2013 | ≤10 |
纬向 | ≤10 |